forcasted 25 degrees. not great for wet-lay

I am pushing to finish the fuel tank moulds today. It’s all wet-lay all the way, and at 25 Centigrade is going to mean a couple of things:

  • hot and sweaty work – I wonder if I can do it outside
  • You can’t mix more than 500ml of resin before it starts to gel off

So, lots of mixing and swearing and sweating. At least cure times will be quick.

Feed the attention-whore